Mosfet multi_layer Moire Lift Hexacontane contact PtfeFilter LeakageCurrent KPFM SThM Non-ContactMode Layer Pinpoint PS_PVAC Metal Vinylpyridine Microchannel GaAs #EC plastics ito_film Adhesive Phenanthrene MultiLayerCeramicCapacitor ThermalProperties solar_cell Glass MonoLayer MeltingPoint Wafer Composition temperature controller AFM Semiconductor EvatecAG PinpointNanomechanicalMode
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Hair
Scanning Conditions
- System: NX10
- Scan Mode: AM-KPFM
- Cantilever: NSC36Cr-Au (k=0.6N/m, f=65kHz)
- Scan Size: 15μm×15μm
- Scan Rate: 0.3Hz
- Pixel: 512×256