biocompatible fluoroaalkane MultiferroicMaterials cannabinoid Stiffness Spincast FFM Bacteria atomic_layer Array strontiu_titanate Fendb CrystalGrowing CeNSE_IISc Piezo Melt Polypropylene Au111 Friction Fiber UnivMaryland CarbonNanotube Boundary IIT-chennai thermoplastic_elastomers MetalCompound WPlug SurfaceOxidation Hafnium_dioxide LateralForce PolyvinylAcetate HACrystal PVAP3HT gallium_nitride Phase
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
CMP test key
Scanning Conditions
- System : NX20
- Scan Mode: Non-contact
- Scan Rate : 1Hz for 25μm2 / 0.6HZ for 15μm2
- Scan Size : 25μm2, 15μm2
- Pixel Size : 512×256 for 25μm2 / 1025×128 for 15μm2