Bmp StyreneBeads silicon_carbide aluminum_nitride Styrene Ni-FeAlloy BoronNitride Self-assembledMonolayer GlassTemp lift_mode CHRYSALIS_INC IRDetector Sio2 Vacuum self_assembly Sidewall Platinum Korea NCM FailureAnalysis AdhesionEnergy Ceramics Magnetic Global_Comm LiftHeight Workfunction HexagonalBN TPU Chemical_Vapor_Deposition SRAM Optoelectronic SSRM Tin sulfide Molybdenum MagneticPhase
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
MoS2 (2/2)
Scanning Conditions
- System: NX10
- Scan Mode: KPFM
- Cantilever: NSC36Cr-Au(k=1N/m, f=90kHz)
- Scan Size: 30μm×30μm,10μm×10μm
- Scan Rate: 0.1Hz
- Pixel: 512×1024