Temperature Gallium_Arsenide Polyaniline AlkaneFilm LiBattery self-assembled_monolayer LeakageCurrent neodymium_magnets PhaseTransition Hair TiO2 Conductance Conductivity margarine exfoliate ElectroDeposition BiVO4 Vacuum Oxide Dimethicone ContactModeDot Biofilm Grain Polyethylene C36H74 temp SmalScan P3HT Mfm Thermoplastic_polyurethane Jason PetruPoni_Institute Fendb VerticalPFM light_emission
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Margarines
Phase change of Margarine surface by temperature control
Scanning Conditions
- System: NX10
- Scan Mode: Tapping, TCS1
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1.2Hz
- Pixel Size: 256 × 256
- Scan Mode: Tapping, TCS1
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1.2Hz
- Pixel Size: 256 × 256