Treatment Writing 2dMaterials Potential Defect Phase Pores Tin sulfide Zhi HighAspect food MolecularSelfAssembly Electronics AM-KPFM HydroGel Conductivity Friction Glass AmplitudeModulation ReflexLens Polydimethylsiloxane GaAs FailureAnalysis 2d_materials Etch Vac C_AFM hydrocarbon ferromagnetic Liquid VinylAlcohol FFM TPU LogAmplifier Stiffness
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
PS/PVAc Film
Film of Polystyrene/poly(vinyl acetate) blend on Si
Scanning Conditions
- System: NX20
- Scan Mode: AM-KPFM
- Cantilever: NSC36Cr-Au C (k=0.6N/m, f=65kHz)
- Scan Size: 15μm×15μm
- Scan Rate: 0.3Hz
- Pixel Size: 1024 × 256
- Scan Mode: AM-KPFM
- Cantilever: NSC36Cr-Au C (k=0.6N/m, f=65kHz)
- Scan Size: 15μm×15μm
- Scan Rate: 0.3Hz
- Pixel Size: 1024 × 256