Strontium Etch VortexCore plastic I-VSpectroscopy AdhesionForce Terrace Zagreb Hexylthiophene molecules PS_LDPE MolybdenumDisulfide Tapping Polyurethane 2dMaterials Carbon Morphology PS_PVAC AAO Oxidation Materials Indium_tin_oxide FFM AtomicLayer Roughness SelfAssembly plastics Ptfe LowDensityPolyethylene LiftMode Nanopattern BTO China fifber Piezoresponse
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Suspended single-layer Graphene
Single-layer Graphene is suspended on microchannels fabricated on Si/SiO2 substrate.
Scanning Conditions
- System: NX20
- Scan Mode: Non-contact
- Cantilever: Access-NC (k=113N/m, f=330kHz)
- Scan Size: 40μm×40μm
- Scan Rate: 0.4Hz
- Pixel Size: 256 × 256
- Scan Mode: Non-contact
- Cantilever: Access-NC (k=113N/m, f=330kHz)
- Scan Size: 40μm×40μm
- Scan Rate: 0.4Hz
- Pixel Size: 256 × 256