Protein Conduct BariumTitanate doped thermal_property self-assembled_monolayer Sio2 HighAcpectRatio Vacuum Thermal ContactModeDot FloppyDisk LDPE Tapping light_emission Silicon Anneal PtfeFilter Genetic PUR cooling MESA structure align ElectroChemical IVSpectroscopy ChemicalCompound ThinFilm Copolymer ElectrostaticForceMicroscopy Wang Crystal Chemical_Vapor_Deposition graphene_hybrid MoirePattern Ecoli
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Pattern in Microchannel
Patterns are used to reduce liquid flow speed in microchannel.
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 3μm×3μm, 5μm×5μm
- Scan Rate:1Hz, 0.5Hz
- Pixel: 512×256, 512×256
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 3μm×3μm, 5μm×5μm
- Scan Rate:1Hz, 0.5Hz
- Pixel: 512×256, 512×256