NiFe Sidewall nanobar AM_KPFM FAFailureAnlaysis Pattern FM_KPFM 2d_materials HexacontaneFilm Ito TemperatureControllerAFM BFO BismuthVanadate Polystyrene Switching temp MagneticForceMicroscopy Domain high_resolution Bmp Nanotechnology PinpointNanomechanicalMode Conduct Cross-section DataStorage ShenYang Hair MultiferroicMaterials Pvdf MolecularSelfAssembly domain_switching HafniumDioxide PvdfBead FM_SKPM Pyroelectric
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
PP/LDPE polymer blend
Scanning Conditions
- System: NX20
- Scan Mode: Pinpoint mechanical
- Cantilever: FMR (k=2N/m, f=75kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.35Hz
- Pixel: 256×256
- Modulus calculation model: Hertzian