HACrystal Celebration CHRYSALIS_INC LithiumNiobate aluminum_nitride MagneticForce Defects Biofilm Hole Ceramics Polarization UTEM single_layer atomic_steps Multiferroic_materials CBD TemperatureControllerStage Mechanical KelvinProbeForceMicroscopy OpticalWaveguides Yeditepe_University Moire lift_mode ContactModeDots FrictionalForceMicroscopy fluorocarbon solar_cell hard_disk_media Perovskite LiftHeight FrequencyModulation amplitude_modulation PvdfFilm ElectroChemical HighResolution
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
TSV Cu pad oxidation
Scanning Conditions
- System : NX-Wafer
- Scan Mode: Non-contact
- Scan Rate : All 1 Hz
- Scan Size : 40μm×40μm
- Pixel Size : All 512×512
- Cantilever : OMCL-AC160TS (k=26N/m, f=300kHz)