Scanning_Thermal_Microscopy Titanate Polymer 3-hexylthiophene Graphite solar_cell fifber AM_SKPM StrontiumTitanate Kevlar SAM LiquidCell NtuEee Yeditepe Techcomp #Materials ThermalDetectors graphene_hybrid HBN HanyangUniv strontiu_titanate FAFailureAnlaysis LogAmplifier fluorocarbon Dental molecules Subhajjit TemperatureControlledAFM Implant LFM Thermal Protein Fet Electronics TungstenDeposition
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Cowpea chlorotic mottle viruses (CCMV)
Scanning Conditions
- System : FX40
- Scan Mode: Tapping in Liquid
- Scan Rate : 3 Hz
- Scan Size : 150nm×150nnm
- Pixel Size : 512×512
- Cantilever : SCOUT 350 (k=42N/m, f=350kHz)