Yeditepe_University IMT_Bucharest molecular_beam Nanostructure PhaseChange Oxidation Transparent Tape CeNSE_IISc Magnetic GranadaUniv SmallScan SoftSample DeflectionOptics MoS2 TCS CHRYSALIS_INC ImideMonomer KPFM FailureAnalysis Pyroelectric Gallium_Arsenide Regensburg YttriaStabilizedZirconia OrganicSemiconductor Photovoltaics Ucl VinylAlcohol AM_KPFM Kevlar cannabidiol TransitionMetal ScanningTunnelingMicroscopy LiNbO3 StrontiumTitanate
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Aligned Fibers
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1Hz
- Pixel Size: 512 × 256
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1Hz
- Pixel Size: 512 × 256