HighAspect Ptfe electrospinning Fendb fe_nd_b Epoxy LiftMode Resistance Solar Chemical Vapor Deposition Chloroform TemperatureControl TyphimuriumBiofilm Regensburg SThM Force-distance Boundary Mechanical&nanotechnology molecules Fujian Nickel ElectroChemical Vacuum LateralForce Display BiasMode FailureAnlaysis PolyvinylAcetate Switching Liquid Annealed SmallScan Non-ContactMode Potential Memory
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
LiNbO3 wafer
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC55TS (k=85N/m, f=1600kHz)
- Scan Size:20μm×20μm, 2.5μm×2.5μm
- Scan Rate: 5Hz, 10Hz
- Pixel: 512×512, 256×256
- Scan Mode: Non-contact
- Cantilever: AC55TS (k=85N/m, f=1600kHz)
- Scan Size:20μm×20μm, 2.5μm×2.5μm
- Scan Rate: 5Hz, 10Hz
- Pixel: 512×512, 256×256