MoS2 H-BN Cobalt-dopedIronOxide PhaseTransition Barium_titanate KAIST Boundary Boron Chromium lithography AEAPDES Memory Conducting Mapping Composite F14H20 Electrical&Electronics LightEmission Scanning_Thermal_Microscopy MESA structure StyreneBeads CancerCell Ferroelectric AdhesionEnergy Granada Etch Nanofiber HighAspect C36H74 Annealing BCZT BismuthVanadate OpticalWaveguide suspended_graphene margarine
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Pattern in Microchannel
Patterns are used to reduce liquid flow speed in microchannel.
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 3μm×3μm, 5μm×5μm
- Scan Rate:1Hz, 0.5Hz
- Pixel: 512×256, 512×256
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 3μm×3μm, 5μm×5μm
- Scan Rate:1Hz, 0.5Hz
- Pixel: 512×256, 512×256