Glass Inorganic_Compound Pores alkanes BismuthVanadate FrictionalForce PolyvinylAcetate BariumTitanate ForceVolumeImage Grain Microchannel MLCC HiVacuum AlkaneFilm Polymer Electronics CalciumHydroxyapatite plastic GranadaUniv Electical&Electronics MolybdenumDisulfide Electrical&Electronics NUS_NNI_Nanocore WS2 SAM Molybdenum_disulfide Modulus Battery Scanning_Thermal_Microscopy BismuthFerrite BiasMode CompactDisk Sadowski Non-ContactMode OpticalModulator
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Cast Iron surface change after Corrosion
Scanning Conditions
- System: NX10
- Scan Mode: Contact
- Cantilever: NSC36C (k=0.6N/m, f=65kHz)
- Scan Size: 50μm×50μm
- Scan Rate: 1.5Hz
- Pixel: 512×1024
- EC bias voltage: -0.266V