KevlarFiber Electronics MeltingPoint LithiumNiobate Chemical_Vapor_Deposition Ni81Fe19 ThinFilm HanyangUniv Fendb WS2 Boundary molecular_beam ferromagnetic PolymerBlend ImideMonomer silicon_oxide Cancer CuFoil TransitionMetal PhaseChange ForceDistanceSpectroscopy Wildtype Silicon INSPParis Tungsten ForceMapping Iron temperature controller AFM Al2O3 HumanHair Crystal PolyStylene atomic_steps Thermal EPFL
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Mo film
Scanning Conditions
- System : NX-Wafer
- Scan Mode: Non-contact
- Scan Rate : 0.5 Hz, 0.8 Hz
- Scan Size : 5μm2, 15μm2
- Pixel Size : All 1024×512
- Cantilever : OMCL-AC160TS (k=26N/m, f=300kHz)