PetruPoni Led HDD tip_bias_mode Moire ULCA PVAC PhaseTransition Aggregated_molecules ElectrostaticForceMicroscopy Laser Polyethylene Electronics Calcium fluorocarbon Vacuum atomic_steps Hafnia Neodymium gallium_nitride MembraneFilter LateralForce Vinylpyridine AM-KPFM Boundary temp_control SFAs ConductingPolymer Treatment Photovoltaics align SolarCell HfO2 Dr.JurekSadowski PpLdpe
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Collagen fibrils
Scanning Conditions
- System : NX10
- Scan Mode: Tapping in Liquid
- Scan Rate : ALL 0.3Hz
- Scan Size : 10μm2, 4μm2
- Pixel Size : ALL 256×256
- Cantilever : PPP-FMR (k=2.8N/m, f=75kHz)