Force-distance BismuthFerrite SiliconeOxide Solution Adhesive LateralForce strontiu_titanate Protein StrontiumTitanate tip_bias_mode LDPE Boundary PS_LDPE HexagonalBoronNitride plastics AdhesionForce Defect HanyangUniv CeramicCapacitor LightEmiting LithiumNiobate Conductance LiftHeight Polyvinylidene Pzt GranadaUniv SingleCrystal Ceramic Chromium DataStorage C_AFM Filter NTU Gong VinylAlcohol
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
C36H74
Layer of C36H74 alkane on HOPG.
Scanning Conditions
- System: NX20
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 256
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 256