Worcester_Polytechnic_Institute Copper Terrace Microchannel Optoelectonics hetero_structure PinpointPFM LightEmiting medical doped SICM Forevision Magnetic Force Microscopy Ecoli Gallium Solar Conducting C36H74 Wafer PhthalocyaninePraseodymium hydrocarbon Subhajjit SicMosfet membrane Ferrite SRAM lift_mode SolarCell Gallium_Arsenide 2dMaterials AM-KPFM Polypropylene INSPParis light_emitting ShenYang
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Cannabidiol(CBD) Molecules
CBD(concentration: 20 mg/mL) molecules assembled on Mica surface after solution rinsing Aggregated CBD molecules as a ring shape.
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 10μm×10μm, 1μm×1μm
- Scan Rate: 0.4Hz, 0.3Hz
- Pixel Size: 512×512, 256×256
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 10μm×10μm, 1μm×1μm
- Scan Rate: 0.4Hz, 0.3Hz
- Pixel Size: 512×512, 256×256