Dimethicone contact Photovoltaics Anneal Genetic Lanthanum_aluminate HafniumDioxide mechanical_property Al2O3 Permalloy non_contact MfmAmplitude Ferroelectric NusEce Scratch thermal_conductivity cannabinoid Magnets DentalProsthesis Conductive AFM ThinFilm tip_bias_mode Etch Austenite Hexylthiophene DiffractiveOpticalElements EFM Molybdenum CrystalGrowing HexacontaneFilm LeakageCurrent FM_SKPM ThermalProperties CVD SicMosfet
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Self-assembly of Semi-fluorinated Alkanes
Domains formed by the self-assembly of semi-fluorinated alkanes deposited as a monolayer on the surface of the water. The monolayer was compressed before being transferred onto a silicon substrate. Each domain includes about 4000 molecules. The domains were easily detached from the substrate with tapping mode because the molecules were very loosely attached to the substrate. Only Non-contact mode could achieve this result.
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: PPP-FMR (k=2.8N/m, f=75kHz)
- Scan Size: 1μm×1μm, 0.5μm×0.5μm, 0.2μm×0.2μm
- Scan Rate: 2Hz
- Pixel Size: 500 × 500
- Scan Mode: Non-contact
- Cantilever: PPP-FMR (k=2.8N/m, f=75kHz)
- Scan Size: 1μm×1μm, 0.5μm×0.5μm, 0.2μm×0.2μm
- Scan Rate: 2Hz
- Pixel Size: 500 × 500