hard_disk_media temperature controller AFM Thermoplastic_polyurethane solar_cell InsulatorFilm light_emission OxideLayer 2d_materials C_AFM Hexacontane PolyimideFilm Filter nanomechanical PolymerBlend HighAcpectRatio NusEce SFAs PolymerPatterns Solar LFM Boundary LiftMode PDMS TemperatureControllerAFM MoS2 Vortex Steps Anneal HBN SiliconeOxide Edwin 2-vinylpyridine Piezo Hafnium_dioxide LowDensityPolyethylene
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
LiNbO3 wafer
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC55TS (k=85N/m, f=1600kHz)
- Scan Size:20μm×20μm, 2.5μm×2.5μm
- Scan Rate: 5Hz, 10Hz
- Pixel: 512×512, 256×256
- Scan Mode: Non-contact
- Cantilever: AC55TS (k=85N/m, f=1600kHz)
- Scan Size:20μm×20μm, 2.5μm×2.5μm
- Scan Rate: 5Hz, 10Hz
- Pixel: 512×512, 256×256