UTEM Memory Perovskite ThermalProperties #EC molecular_beam BiasMode Blood HafniumDioxide self_assembly Conduct TipBiasMode Regensburg Deposition AM-KPFM temperature controller AFM Tungsten_disulfide Hole membrane DeflectionOptics biocompatible Current Gong BariumTitanate SrTiO3 Aggregated_molecules PVA MLCC Dimethicone Beads Gallium_Arsenide Fujian Singapore PolycrystallineFerroelectricBCZT Chromium
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Hydro gel
Scanning Conditions
- System: NX10
- Scan Mode: NCM, Liquid mode
- Cantilever: BL-AC40 (k=0.1N/m, f=110kHz)
- Scan Size: 50μm×50μm
- Scan Rate: 1Hz
- Pixel: 512×256