Hole Wonseok ImideMonomer NanoLithography STM OpticalModulator PVAC DentalProsthesis Conductive AFM Perovskite Bismuth fifber SrO UTEM Silver lithography MolybdenumDisulfide AM_SKPM MoS2 semifluorinated_alkane Self-assembledMonolayer SiWafer FrictionalForceMicroscopy CrAu Genetic SICM ForceVolumeImage organic_polymer Hexatriacontane Patterns GaAs China plastics Tungsten_disulfide Heating
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Defects of Reflex lens
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel: 512×512