Barium_titanate Mechanical&nanotechnology Indium_tin_oxide TemperatureControllerStage MagneticArray lift_mode EFMAmplitude Pore SiliconCrystal MechanicalProperties PinpointNanomechanicalMode PolycrystallineFerroelectricBCZT temp_control Titanate Optical Yeditepe_University Conductivity temp Chloroform FrictionalForce BismuthFerrite LiquidCell GaN Galfenol Bismuth LDPE Wang HexagonalBoronNitride SKPM Conducting polymeric_arrays KAIST Edwin Varistor CaMnO3
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Magnetic device
Scanning Conditions
- System : NX20
- Lift Height : 50nm
- Scan Mode: MFM
- Scan Rate : 0.3Hz
- Scan Size : 20μm×20μm
- Pixel Size : 512×256
- Cantilever : PPP-MFMR (k=2.8N/m, f=75kHz)