CuFoil LiftHeight KAIST Polypropylene CancerCell PolyvinylideneFluoride Grain SingleCrystal Mapping BaTiO3 ScanningSpreadingResistanceMicroscopy MechanicalProperty membrane cannabinoid ThermalConductivity graphene_hybrid Temperature Etch light_emission conductive Al2O3 DeflectionOptics MagneticForce Defect Titanate PhaseChange MagneticPhase Magnetic Force Microscopy PolyStylene Ceramics Metal-organicComplex Implant FrictionalForceMicroscopy LiftMode Annealing
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Triple-cation perovskite
Scanning Conditions
- System : NX10
- Sample bias: 0 V, 0.5 V
- Scan Mode: C-AFM with PCM toolkit
- Scan Rate : 0.25 Hz
- Scan Size : 5μm×5μm
- Pixel Size : 512×512
- Cantilever : ANSCM-PC (k=0.2N/m, f=12kHz)