dielectric trench multi_layer Yeditepe_University PhaseTransition AEAPDES fifber Tin sulfide UnivCollegeLondon Pores Corrosion fluoroaalkane Pzt TappingMode DeoxyribonucleicAcid GaP Dental BTO StyreneBeads Ferroelectric China Gallium LMF Stiffness SFAs BCZT Lateral Granada PatternedSapphireSubstrat Strontium ElectrostaticForceMicroscopy InLiquid Pattern block_copolymer BFO Titanate
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
MoS₂ film
Scanning Conditions
- System : FX40
- Scan Mode: Tapping
- Scan Rate : 1Hz
- Scan Size : 40μm×40μm
- Pixel Size : 512×256
- Cantilever : OMCL-AC160TS (k=26N/m, f=300kHz)