OpticalElement BismuthVanadate Spain Materials Galfenol MagneticArray Pzt NUSNNI NUS SingleCrystal frequency_modulation Reading dielectric trench UnivOfMaryland Formamidinium_lead_iodide HBN Temperature MultiLayerCeramicCapacitor Ecoli Composition ContactModeDots CNT Optoelectronic HafniumDioxide HydroGel IIT-chennai UnivMaryland tip_bias_mode MagneticForce VerticalPFM PvdfBead HighAcpectRatio Platinum Conductance Graphite
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Moire pattern of MoS₂-WSe₂
Scanning Conditions
- System : FX40
- Scan Mode: Tapping
- Scan Rate : 3Hz
- Scan Size : 500nm×500nm
- Pixel Size : 512×512
- Cantilever : PPP-FMR (k=2.8N/m, f=75kHz)