CrAu SiWafer Optic TempControl TemperatureControllerStage Oxidation OrganicSemiconductor Ram BiFeO3 CeNSE_IISc Genetic Mechanical&nanotechnology TransitionMetal DentalProsthesis Ucl TungstenDeposition Hafnia LaAlO3 Tapping Blend BariumTitanate Led DNAProtein Ferrite Vinylpyridine Lateral_Force_Microscopy PVAP3HT Indent Electrode FrictionForce CHRYSALIS_INC Regensburg NCM\ PANI AM_SKPM
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
F14H20
Semifluorinated alkanes on Si.
Scanning Conditions
- System: NX20
- Scan Mode: Tapping
- Cantilever: AD40AS (k=40N/m, f=180kHz)
- Scan Size: 5μm×5μm, 1μm×1μm
- Scan Rate: 05Hz, 1Hz
- Pixel Size: 1024 × 512, 512 x 256