GalliumPhosphide lithography Nickel Deposition CrAu CuFoil Adhesion PhaseTransition sputter MechanicalProperty Fet TriGlycineSulphate OrganicCompound FuelCell Dopped Defect ULCA GaAs AdhesionForce CntFilm PVAP3HT food MLCC ScanningTunnelingMicroscopy Copolymer Leakage Laser ScanningIon-ConductanceMicroscopy LateralPFM Modulus AM-KPFM BismuthFerrite atomic_layer multi_layer DomainSwitching
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Formamidinium Lead Iodide FAPbI3 Perovskite Film
FAPbI3 is an organic-inorganic hybrid perovskite material for nowadays high efficiency perovskite solar cell.
Scanning Conditions
- System: NX10
- Scan Mode: Conductive AFM
- Cantilever: CDT-NCHR (k=80N/m, f=400kHz)
- Scan Size: 15μm×15μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 256
- Scan Mode: Conductive AFM
- Cantilever: CDT-NCHR (k=80N/m, f=400kHz)
- Scan Size: 15μm×15μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 256