Chemical_Vapor_Deposition Optoelectonics WPlug Sulfur ChemicalCompound Holes AlkaneFilm Worcester_Polytechnic_Institute PolyStylene Reduction IISCBangalore DNA OpticalElement Piezo Piezoresponse Patterns RedBloodCell norganic BismuthFerrite Platinum Conductivity Water DomainSwitching Bacterium PiezoelectricForceMicroscopy Flake SmallScan FM_KPFM Magnetostrictive CaMnO3 Protein NUS NusEce AmplitudeModulation ito_film
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
PS/PVAc Film
Film of Polystyrene/poly(vinyl acetate) blend on Si
Scanning Conditions
- System: NX20
- Scan Mode: AM-KPFM
- Cantilever: NSC36Cr-Au C (k=0.6N/m, f=65kHz)
- Scan Size: 15μm×15μm
- Scan Rate: 0.3Hz
- Pixel Size: 1024 × 256
- Scan Mode: AM-KPFM
- Cantilever: NSC36Cr-Au C (k=0.6N/m, f=65kHz)
- Scan Size: 15μm×15μm
- Scan Rate: 0.3Hz
- Pixel Size: 1024 × 256