Praseodymium Nanostructure Boron Molybdenum Sapphire Composition ring shape conductive ShenYang INSPParis PolymerBlend Pinpoint BiVO4 Al2O3 LiIonBattery Force-distance PMNPT NUS_Physics DeflectionOptics SThM Ito Polydimethylsiloxane FastScan 3-hexylthiophene Spincast Aggregated_molecules Annealed thermal_conductivity ElectroChemical Hydroxyapatite Au111 NusEce Plug Defects Ceramic
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Hard Disk Media
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: SSS-NCHR (k=42N/m, f=300kHz)
- Scan Size: 1μm×1μm, 0.3μm×0.3μm
- Scan Rate: 0.5Hz, 1Hz
- Pixel Size: 512×512, 256×256
- Scan Mode: Non-contact
- Cantilever: SSS-NCHR (k=42N/m, f=300kHz)
- Scan Size: 1μm×1μm, 0.3μm×0.3μm
- Scan Rate: 0.5Hz, 1Hz
- Pixel Size: 512×512, 256×256