ForceVolume NiFe Glass Austenite Stiffness LaAlO3 SiWafer Fet BCZT Annealed PhaseTransition ScratchMode Wang MagneticForceMicroscopy OrganicSemiconductor YszSubstrate TemperatureControlledAFM AEAPDES Oxide Cross-section norganic SAM Butterfly SingleCrystal FM_KPFM Electronics DataStorage WS2 LiftHeight Spincast HighAspect Galfenol TPU SFAs hetero_structure
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Calcite surface change in Ca(OH)2
Scanning Conditions
- System: NX20
- Scan Mode: Universal liquid cell, Contact mode
- Cantilever: BL-AC40TS
- Scan Size: 45μm×45μm, 0.5μm×0.5μm
- Scan Rate: 3Hz
- Sample: Iceland spar (calcite)
- React Solution Ca(OH)2
- Pixel: 512 × 256, 256 × 256
- Scan Mode: Universal liquid cell, Contact mode
- Cantilever: BL-AC40TS
- Scan Size: 45μm×45μm, 0.5μm×0.5μm
- Scan Rate: 3Hz
- Sample: Iceland spar (calcite)
- React Solution Ca(OH)2
- Pixel: 512 × 256, 256 × 256