Optoelectronic plastic FM-KPFM PrCurve Insulator CntFilm Butterfly StrontiuTitanate dielectric_trench Steps PVA AdhesionForce BlockCopolymer Sapphire Writing Polystyrene MagneticPhase block_copolymer Organic PECurve aluminum_nitride InLiquid Fe_film Iron Optical CuFoil ContactModeDots Cancer Electical&Electronics Polypropylene FrictionalForce Leakage PatternedSapphireSubstrat TemperatureControlledAFM CHRYSALIS_INC
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
BN thin film on Si
Scanning Conditions
- System: NX10
- Scan Mode:SThM
- Cantilever: Nanothermal probe
- Scan Size: 25μm×25μm, 5μm×5μm
- Scan Rate:0.3Hz, 0.5Hz
- Pixel: 256×256, 256×256
- Scan Mode:SThM
- Cantilever: Nanothermal probe
- Scan Size: 25μm×25μm, 5μm×5μm
- Scan Rate:0.3Hz, 0.5Hz
- Pixel: 256×256, 256×256