PtfeFilter Permalloy ForceDistanceSpectroscopy AEAPDES Anneal Hafnium_dioxide plastics Wonseok NUS_Physics Bacterium MagneticPhase TipBiasMode AM_KPFM Edwin SetpointMode NUSNNI Thermoplastic_polyurethane SThM Carbon hetero_structure LateralPFM MBE MoS2 Nickel ThermalDetectors Croatia Hysteresys PMNPT Galfenol FastScan 3-hexylthiophene rubber PtfeMembrane Polypropylene Treatment
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Block copolymer Ι
Scanning Conditions
- System: NX20
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.8Hz
- Pixel: 512×512
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.8Hz
- Pixel: 512×512