GaN TemperatureControllerAFM Filter Mosfet Ca10(PO4)6(OH)2 OpticalWaveguides Bacteria mechanical_property TCS Inorganic LiIonBattery non_contact DOE #EC Bacterium UnivMaryland WS2 CuFoil ito_film Aluminium_Oxide semifluorinated_alkane PolyimideFilm Boundary Flake Monisha MeltingPoint AM_KPFM Polystyrene gallium_nitride TransitionMetal HOPG strontiu_titanate Ucl MolecularSelfAssembly Potential
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Calcium Hydroxyapatite Crystal growing
HA crystal grows according to the annealing time. From 24hrs, the crystal becomes clearly.
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 1μm×1μm
- Scan Rate: 0.17Hz
- Pixel: 512×256
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 1μm×1μm
- Scan Rate: 0.17Hz
- Pixel: 512×256