EFMAmplitude IVSpectroscopy StyreneBeads PetruPoni_Institute Step PinpointNanomechanicalMode CBD Holes fluorocarbon Lateral_Force_Microscopy DomainSwitching ito_film heterojunctions temperature_control Display SKPM DeoxyribonucleicAcid suspended_graphene Praseodymium Potential AtomicLayer HDD PhaseImaging Copper PvdfFilm membrane MagneticPhase EFM NtuEee Glass MultiLayerCeramicCapacitor Polystyrene RedBloodCell IndiumTinOxide Ito
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Domain switching on PZT
Scanning Conditions
- System: NX10
- Scan Mode: Lithography, PFM
- Cantilever: ContscPt (k=0.2N/m, f=25kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel: 512×512
- Litho. mode: Tip bias mode
- Litho. Tip bias: Black +10V, White -10V