epitaxy LiquidCrystal Filter HOPG CVD LiNbO3 Workfunction fluoroaalkane CrystalGrowing SrO Liquid ForceMapping PDMS DOE molecule Modulus atomic_layer Dental Scanning_Thermal_Microscopy Crystal HexacontaneFilm HiVacuum FM-KPFM Praseodymium Ptfe temperature controller AFM ShenYang SICM Vortex cannabis Domain Vac CalciumHydroxide PetruPoni Inorganic_Compound
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Styrene beads
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 2μm×2μm
- Scan Rate: 0.5Hz
- Pixel: 512×512