SiliconeOxide Hafnium_dioxide Melt InLiquid EFM CHRYSALIS_INC Polyethylene Granada Chungnam_National_University ScanningIon-ConductanceMicroscopy Workfunction SKKU molecule NiFe PVA DOE Pyroelectric Lattice IndiumTinOxide cannabidiol ContactModeDots Calcite 2d_materials HexagonalBoronNitride AnodizedAluminumOxide Patterns AEAPDES FM_KPFM Pores margarine HBN TipBiasMode Composite Morphology epitaxy
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Ferroelectric superlattices in 2L-hBN (0°)
Scanning Conditions
- System : FX40
- Scan Mode: Sideband KPFM
- Scan Rate : All 0.3 Hz
- Scan Size : 3μm×3μm, 4μm×4μm
- Pixel Size : All 512×512
- Cantilever : ElectricMulti75-G (k=3N/m, f=75kHz)