TempControl Wonseok Mosfet BiVO4 hydrocarbon Composite HighResolution PECurve #Materials Mfm MagneticPhase epitaxy AM_SKPM Holes Molybdenum LateralPFM EPFL Mechinical fluorocarbon Protein AtomicLayer Composition nanomechanical IISCBangalore Spain Device Ito PolymerPatterns Etch semifluorinated_alkane TappingMode lift_mode thermal_conductivity HydroGel polymeric_arrays
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Fractals of silver nanoparticles
Scanning Conditions
- System : NX10
- Scan Mode: Non-contact
- Scan Rate : 0.31 Hz, 0.27 Hz
- Scan Size : 50μm2, 40μm2
- Pixel Size : All 256×256
- Cantilever : OMCL-AC160TS (k=26N/m, f=300kHz)