Boundary Temasek_Lab StyreneBeads 2dMaterials non_contact LateralForceMicroscopy AM-KPFM ItoGlass ImideMonomer Biology Etch Bmp HydroGel Gallium_Arsenide SrTiO3 DLaTGS Wang Microchannel YszSubstrate atomic_layer Oxidation Zagreb hard_disk_media FrictionalForce Cross-section KelvinProbeForceMicroscopy food Polypropylene CompactDisk SmallScan Pvdf Modulus Lift Vacuum IIT-chennai
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
AR Lens
Scanning Conditions
- System : FX40
- Scan Mode: Non-contact
- Scan Rate : 0.5 Hz for 40μm2, 1.5 Hz for 5μm2, 2μm2
- Scan Size : 40μm2, 5μm2, 2μm2
- Pixel Size : 2048×512 for 40μm2, 5μm2, 1024×256 for 2μm2
- Cantilever : OMCL-AC55TS (k=85N/m, f=1.6kHz)