NCM cannabidiol PiezoelectricForceMicroscopy dielectric trench Sphere Chemical_Vapor_Deposition Croatia Alkane Protein Hydroxyapatite AM_SKPM PinpointNanomechanicalMode Imprint Metal-organicComplex Lanthanum_aluminate semifluorinated_alkane Korea LiquidCrystal block_copolymer Stiffness Phosphide Fet Implant Chrome Yttria_stabilized_Zirconia DeflectionOptics Sulfur Praseodymium 2dMaterials WWafer LiquidCell plastic Annealed PECurve Resistance
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Nanostructures on polymer
Scanning Conditions
- System : NX10
- Scan Mode: Non-contact
- Scan Rate : 0.5 Hz
- Scan Size : 5μm×5μm
- Pixel Size : 256×256
- Cantilever : PPP-NCHR (k=42N/m, f=330kHz)