mono_layer EvatecAG Mapping Fendb MembraneFilter Ananth CopperFoil EPFL Nanopattern H-BN ito_film cannabidiol LeakageCurrent TemperatureControllerStage Friction Current Chloroform cannabinoid Bmp Resistance Fluoride Genetic PatternedSapphireSubstrat Mechanical&nanotechnology temperature controller AFM Ptfe ScanningThermalMicroscopy 3-hexylthiophene HOPG ULCA SKKU silicon_carbide Mechanical polymeric_arrays Polarization
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Fe-Nd-B Alloy
Scanning Conditions
- System: NX10
- Scan Mode: MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 15μm×15μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 256
- Lift height: 100nm
- Scan Mode: MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 15μm×15μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 256
- Lift height: 100nm