Bacterium Domain norganic LiftHeight Inorganic Conducting Non-ContactMode MfmPhase self-assembled_monolayer Techcomp vertical_PFM Bio Oxidation DOE ThermalDetectors atomic_steps Heating NanoLithography Polymer nanomechanical SRAM ScanningThermalMicroscopy CrossSection Electronics HydroGel Fe_film ContactModeDots Metal MolecularSelfAssembly DeoxyribonucleicAcid Sidewall ScanningTunnelingMicroscopy Vac Piezoelectric Annealed
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Al2O3-doped CaMnO3
1% Al2O3-doped CaMnO3 on LaAlO3 (001) orientation substrate by pulsed laser deposition.
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1Hz
- Pixel Size: 256 × 256
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1Hz
- Pixel Size: 256 × 256