SiliconeOxide cannabinoid Polyvinylidene_fluoride PVAC MechanicalProperty Conductivity ElectrostaticForceMicroscopy ferromagnetic Permalloy Oxidation PpLdpe Metal FM_SKPM AlkaneFilm GlassTemperature AdhesionForce thermoplastic_elastomers self-assembly sputter Tungsten_disulfide YttriaStabilizedZirconia Pvdf LithiumNiobate Bmp cannabidiol PUR Chromium self-assembled_monolayer Silicon HanyangUniv PiezoelectricForceMicroscopy rubber Tungsten SKKU I-VSpectroscopy
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
HfO2 into Indium Tin Oxide Film
ITO film on 1% HfO2-doped Yttria-stabilized Zirconia (001) orientation grown by pulsed laser deposition. Surface segregation of HfO2 into ITO film.
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz))
- Scan Size: 10μm×10μm,5μm×5μm
- Scan Rate: 0.6Hz, 1Hz
- Pixel Size: 256 × 256, 256 x 256
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz))
- Scan Size: 10μm×10μm,5μm×5μm
- Scan Rate: 0.6Hz, 1Hz
- Pixel Size: 256 × 256, 256 x 256