BoronNitride Biology Polytetrafluoroethylene PS_LDPE Phosphide Reading Inorganic NTU 2d_materials Deposition Glass Adhesive Polyaniline ring shape MetalCompound UTEM MagneticArray FFM Change Silicon Flake Korea TyphimuriumBiofilm amplitude_modulation Solar TappingMode BiFeO3 Logo Scratch C_AFM Granada 2dMaterials Monisha SICM DNAProtein
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Polymer blend with nanofiber
Scanning Conditions
- System: NX10
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.5Hz
- Pixel: 512×512
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.5Hz
- Pixel: 512×512