hetero_structure PVAC LiquidCrystal Foil Vacuum Ca10(PO4)6(OH)2 tip_bias_mode Reduction ShenYang ForceDistanceSpectroscopy Thermal Magnetic Force Microscopy nanomechanical CrystalGrowing rubber Holes MolecularSelfAssembly SKKU Conductance Gallium_Arsenide BiasMode CntFilm China TappingMode mechanical_property HexacontaneFilm Boron LeakageCurrent Spain thermal_property HighResolution Bmp Ucl Tungsten VinylAlcohol
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
ITO glass
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 3μm×3μm, 1μm×1μm
- Scan Rate: 0.4Hz, 1Hz
- Pixel: 512×512, 512×512