Magnets SingleCrystal ScanningTunnelingMicroscopy Collagen Tin disulfide IISCBangalore hard_disk oxide_layer Flake Vac MBE PhaseChange BaTiO3 Optoelectronic ScratchMode Formamidinium_lead_iodide OpticalWaveguide LiNbO3 polyvinyl acetate small_scan OpticalWaveguides SiliconCrystal fifber MagneticForceMicroscopy NusEce TemperatureControllerAFM Ni-FeAlloy Dopped CancerCell HfO2 LiftMode MESA structure Display LDPE PolyvinylideneFluoride
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Styrene beads
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 2μm×2μm
- Scan Rate: 0.5Hz
- Pixel: 512×512