Chemical_Vapor_Deposition Modulus neodymium_magnets Polyimide Fe_film IVSpectroscopy KAIST doped LFM AmplitudeModulation MechanicalProperty ferromagnetic Phthalocyanine fifber HardDisk PVAP3HT Dopped ContactMode Solar Barium_titanate Bismuth SKPM ScanningSpreadingResistanceMicroscopy Singapore GalliumPhosphide Praseodymium PolyStylene contact Polytetrafluoroethylene Non-ContactMode AtomicSteps pulsed_laser_deposition FM_KPFM SRAM HighAcpectRatio
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
HOPG
Scanning Conditions
- System : FX40
- Scan Mode: Sideband, AM KPFM
- Scan Rate : 0.55 Hz
- Scan Size : 10μm×10μm
- Pixel Size : 256×256
- Cantilever : NSC36 Cr-Au C (k=0.6N/m, f=65kHz)