semifluorinated alkane mfm_amplitude Ram STO Adhesion PUR blended polymers CVD 3-hexylthiophene GaN Perovskite MagneticArray silicon_oxide ScanningKelvinProbeMicroscopy fluoroalkane PDMS Fiber Typhimurium Piranha Vac KelvinProbeForceMicroscopy Ito Plug AAO CuSubstrate ContactModeDots Collagen pinpoint mode LightEmiting Bmp temp Step Neodymium IMT_Bucharest Polyaniline
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Semi-fluorinated alkanes
Scanning Conditions
- System : NX10
- Scan Mode: Sideband KPFM
- Scan Rate : 0.4 Hz
- Scan Size : 500nm×500nm
- Pixel Size : 256×256
- Cantilever : HQ: NSC14/CR-AU (k=5N/m, f=160kHz)