LiquidCrystal Semiconductor strontiu_titanate WWafer HfO2 SoftSample Butterfly ito_film Christmas IcelandSpar AM_SKPM NtuEee IMT_Bucharest PetruPoni piezoelectric force microscopy cooling nanomechanical Subhajjit ForceDistanceSpectroscopy Optic TemperatureControllerAFM Etch MLCC LogAmplifier Battery ReflexLens Polyaniline BaTiO3 EvatecAG Nanotechnology Materials suspended_graphene Typhimurium LiquidImaging self-assembled_monolayer
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Crosslinked starch & pectin fibers
Scanning Conditions
- System : NX-Wafer
- Scan Mode: Tapping
- Scan Rate : 0.31 Hz
- Scan Size : 15μm×15μm
- Pixel Size : 256×256
- Cantilever : ContSCR (k=0.2N/m, f=25kHz)