Polyvinylidene BreastCancerCell Chromium AtomicSteps DOE PyroelectricDetector PhaseImaging HardDiskMedia ScratchMode Polyvinylidene_fluoride solar_cell Hole dielectric_trench Semiconductor StyreneBeads Yttria_stabilized_Zirconia Boron NUSNNI InorganicCompound NusEce plastic ElectroChemical small_scan TiO2 HiVacuum Optoelectonics organic_polymer Change IIT-chennai Cell LiquidCell FFM Conducting SelfAssembly EFMAmplitude
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Nanostructures on polymer
Scanning Conditions
- System : NX10
- Scan Mode: Non-contact
- Scan Rate : 0.5 Hz
- Scan Size : 5μm×5μm
- Pixel Size : 256×256
- Cantilever : PPP-NCHR (k=42N/m, f=330kHz)